Description
CPM S90-V
Note: All steel is sold by the foot. When picking the quantity of 2, equals a 2 foot bar. CPM steels are in 3 foot lengths. Please provide your cutting instructions in the shopping cart left of the total price in the box “Special instructions for seller”. If no instructions are provided, we cut based on the following:
2 foot lengths will ship in 2 foot lengths.
3 foot lengths will ship in 3 foot lengths.
5 foot order will be shipped in a 2 foot and 3 foot length.
CPM S90-V is a unique tool steel made by the Crucible, a martensitic stainless steel with a high volume of vanadium carbides means a blade with exceptionally good wear resistance and wicked sharp edges.
S90V offers substantial improvements in wear resistance over other high chromium tool steels, such as D2, and corrosion resistance on par or above most 440C type steels.
These attributes are the byproduct of its high volume of vanadium carbides to chromium carbides, where one adds wear resistance, the chromium in the matrix provides good corrosion resistance.
A favorite among folder and kitchen knife makers, S90-V is known for taking an exceptional satin finish to match its excellent edge retention properties.
CPM S90V stainless steel at a glance
- Steel type: High-vanadium powder-metallurgy (CPM) stainless steel.
- Typical chemistry: C 2.30, Cr 14.0, V 9.0, Mo 1.0 (%)
- Thicknesses: 3/32″ and 1/8″
- Widths: 1.5″ and 2″
- Length: Sold by the foot from 3-foot bars.
- Good for: Maximum edge retention in folders and kitchen knives. Expect slow grinding.
How to heat treat CPM S90V stainless steel
These starting points come from Niagara Specialty Metals (the Crucible CPM data sheet)’s published data sheet. Results depend on your kiln, quench and blade thickness, so check hardness on a test piece first.
- Harden: 2,100–2,150°F (1,150–1,175°C), hold 20 minutes.
- Quench: Plate or positive-pressure quench, cooling at least 150°F (80°C) per minute to below 1,000°F (540°C), then to below 125°F (50°C) before tempering.
- Cryo: Optional, between the first and second temper. Always temper after it.
- Temper: Twice at 400–750°F (200–400°C), at least 2 hours each. Avoid 800–1,000°F (425–540°C), which reduces corrosion resistance.
Full data sheet: CPM S90V stainless steel heat-treat data sheet (PDF). More grades are on our Heat Treating Data page.
Supplies we stock for this steel: 309 stainless tool wrap to protect blades from scale at hardening temperature, ATP-641 anti-scale coating and Evenheat kilns.
Safety: liquid nitrogen and dry ice cause severe cold burns. Wear insulated gloves and eye protection, and work in a ventilated space.











Reviews
There are no reviews yet